[Prev][Next][Index][Thread]

Re: ,)




>>What dialectric did you use? 1 0.060 polyethylene like I did as an expediant
>>method, or 3 0.030" layer like Richard Quick recomends?
>>
>>                                jim
>>
>>
>
>I used the 0.060 polyethylene.  I got it from a plastics company in
>Sacramento.
>How long did you let them soak before you used them?
>
>
>Mark R. Napier
>napier-at-cats.ucsc.edu
>
I let it soak about 1/2 an hour after I pulled a vacuum on it. It bubbled
quit nicely for about 5 minutes under vacuum before the top lid cracked. My
next cap will use 3/16" plexiglass as endcaps.