>Hello all,
>I was wondering if anyone has tried this I am going to wind a new secondary
>using pvc and cover it with a heat shrink plastic that has a heat activated
>adhesive known as Monokote and other brand names, used to cover radio
>control airplanes. I am not sure but I think this mylar. Would this take the
>place of painting it with a sealer? Monokote is easy to work with even more
>so if you have a heat gun. Thanks
>
>Brad McPeak
>
Hello Brad,
Haven't seen you in a while!
Heat shrink plastic - been there, tried it. I got sparks which traveled
down between the windings. It looked like they followed the plastic,
between it and the insulation on the wire. I immediately took the heat
shrink plastic off.
Sorry, it does not work worth a hoot.