[Prev][Next][Index][Thread]
Re: Caps.
>Original Poster: "Bunnykiller" <bigfoo39-at-telocity-dot-com>
>
>Tesla List wrote:
>>
>> Original Poster: "Charles Arruda" <carruda-at-channelseek-dot-com>
>>
>> Has anyone tried to make a cap with a really nice powdered dielectric
>> (High K) like Barium Titanate? BaTi has an K factor of about 1,200
>> compared to other materials that are around 6-12.
>
>
>Snipppp
>
>
>Hi Charles...
>
>ever price Barium Titanate? it does come in a ceramic form but good
>gawd its pricey.... a 1/16" thick 12X12 sheet runs approximately 170$
>I'd rather buy virgin teflon ;) ...
>
>
>Scot D
>
>
Or you buy the powder from micronmetals for $25.09 per pound.
Do you have a very hot oven?
Ruud de Graaf
Greetings from Holland