[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
Re: Pre-catalyzed lacquer for secondary
Original poster: "teri mckenney by way of Terry Fritz <twftesla-at-uswest-dot-net>" <mck-at-ezy-dot-net>
----- Original Message -----
From: Tesla list <tesla-at-pupman-dot-com>
To: <tesla-at-pupman-dot-com>
Sent: Thursday, April 26, 2001 7:06 AM
Subject: Pre-catalyzed lacquer for secondary
> Original poster: "teri mckenney by way of Terry Fritz
<twftesla-at-uswest-dot-net>" <mck-at-ezy-dot-net>
>
> Hello all,
> Just getting ready to wrap my secondary and was think'in of coating it
with
> pre-catalyzed lacquer.It can be applied in literally seconds with a HVLP
> sprayer and cures in 10-15 minutes.The fast curing time eliminates sags
and
> runs and dramatically reduces dust and bugs.P.C. lacquer is a conversion
> varnish that has lacquer resins added.It cures much the same as
polyurethane
> and varnish in that the resins crosslink thus eliminating the problem of
> plasticizer migration so common with regular lacquer.If U.V. is a major
problem
> maybe a final coat of marine varnish.Think it will be allright?